Plate applications
Indoor equipment panels, appliance trim, formed covers and other mildly corrosive applications where magnetic behavior and finish are relevant.
REQUEST A QUOTE
Send the details you already know. Our team can review the remaining technical points with you.
Plate · Grade 430 / S43000
430 stainless steel plate is a ferritic chromium grade used where moderate corrosion resistance, oxidation resistance and low thermal expansion are useful. Confirm that the ordered thickness is available as plate and state ASTM A240/A480 edition, condition, finish, dimensions and inspection.

Send the service environment, finish and thickness for a 430 plate review.
Indoor equipment panels, appliance trim, formed covers and other mildly corrosive applications where magnetic behavior and finish are relevant.
Do not assume 430 provides 304/316-level chloride resistance or weld performance. Strongly corrosive, marine or crevice service needs a project-specific alternative review.
UNS S43000; EN 1.4016. Verify the ordered product standard and certificate.
Chemistry and physical properties are grade references. Mechanical values are ATI sheet/strip data and are not represented as plate-specific acceptance limits.
ATI 430 composition limits are shown as a grade reference. Confirm the ordered plate specification, edition and heat analysis. ATI publishes 450 MPa tensile, 205 MPa yield, 22% elongation and 89 HRB maximum for 430 sheet/strip. These values are material-screening references only; plate acceptance depends on thickness, condition and the ordered ASTM A240/A480 edition.
| Element | Minimum | Maximum | Unit |
|---|---|---|---|
| Cr | 16.0 | 18.0 | wt % |
| Si | N/A | 1.00 | wt % |
| Mn | N/A | 1.00 | wt % |
| Ni | N/A | 0.75 | wt % |
| C | N/A | 0.12 | wt % |
| P | N/A | 0.040 | wt % |
| S | N/A | 0.030 | wt % |
| Fe | Balance | N/A | wt % |
| Property | Minimum | Maximum / range | Unit | Condition / reference |
|---|---|---|---|---|
| Tensile strength | 450 | N/A | MPa | ATI 430 sheet/strip; published minimum. Screening reference for a plate enquiry only. |
| 0.2% proof / yield strength | 205 | N/A | MPa | ATI 430 sheet/strip; published minimum. Screening reference for a plate enquiry only. |
| Elongation | 22 | N/A | % | ATI 430 sheet/strip; 22% published minimum; ATI notes 20% minimum at 1.27 mm and under. Screening reference for a plate enquiry only. |
| Hardness | N/A | 89 | HRB | ATI 430 sheet/strip; published maximum. Screening reference for a plate enquiry only. |
| Property | Published value | Basis / note |
|---|---|---|
| Density | 7.70 g/cm³ | ATI 430 typical physical property; density |
| Linear thermal expansion (20–100°C) | 10.3 × 10⁻⁶ /°C | ATI 430 typical value; stated temperature range |
| Thermal conductivity (20–100°C) | 23.86 W/(m·K) | ATI 430 typical value; stated temperature range |
| Specific heat (0–100°C) | 460 J/(kg·K) | ATI 430 typical value; stated temperature range |
Data note: These values are material-screening references. The governing product specification, ordered condition, dimensions and heat-specific certificate determine acceptance. Review the technical resources for the applicable purchasing basis.

State thickness, width × length, finish, temper, edge, flatness and tolerances. Verify 430 plate sizes against the order basis and the chosen finish. When comparing a 430 plate supplier, require a 430 plate specification to ASTM A240, finish callout, certificate and dimensional tolerances. For an ASTM 430 plate enquiry, cite ASTM A240 and confirm finish, thickness and dimensional tolerances on the order.
| Duty / item | Starting option | Advantage | Limitation | Alternative / action |
|---|---|---|---|---|
| Appliance panel | 430 plate to specified finish and thickness | Magnetic ferritic grade can suit formed trim | Check finish direction and forming radius | Run a bend trial at the stated radius and grain direction |
| Equipment cover | 430 plate after cleaner and chloride review | Plate form supports bends and covers | Avoid chloride traps and wet crevices | Compare 304 where exposure or cleaning severity exceeds 430 margin |
| Decorative trim | 430 plate with approved surface finish | Finish options affect appearance | Color and grain vary by lot and process | Approve a lot-specific finish sample before production |
Product standard: ASTM A240/A240M covers stainless plate, sheet and strip; ASTM A480/A480M supplies general flat-rolled requirements. State 430/S43000, edition, plate dimensions, condition, finish and supplements.
Finish and condition: Specify finish direction, protective film, edge quality and forming condition. Review the approved appearance sample and avoid iron contamination.
Order checks: confirm exact dimensional basis, tolerance, finish, edge/end preparation, quantity and delivery requirements before quotation.
Discuss plate application; send the grade, product dimensions and service conditions.
430 stainless steel plate is a ferritic chromium stainless option for applications prioritizing magnetic response, formability and general atmospheric corrosion resistance. Specify thickness, finish, flatness, edge, temper and standard; do not treat 430 as a substitute for molybdenum-bearing grades in chloride exposure. Do not assume 430 provides 304/316-level chloride resistance or weld performance. Strongly corrosive, marine or crevice service needs a project-specific alternative review.
| Failure mode | Typical trigger | Control / verification |
|---|---|---|
| Chloride pitting or staining | Salt, chloride-bearing moisture, deposits or stagnant crevices can exceed the corrosion margin of ferritic 430. | Review chloride concentration, temperature and cleaning; avoid stagnant deposits and consider a more corrosion-resistant grade for severe exposure. |
| Visible finish mismatch | Finish, grain direction, handling marks or protective-film expectations are not defined consistently. | Specify finish and grain direction, edge condition and protective packaging; inspect sample and delivered lot against the agreed appearance criteria. |
| Forming cracks or surface damage | Tight bend radii, high strain, tooling condition or an unsuitable material condition can damage formed plate. | Confirm condition, thickness and bend direction; validate tooling and bend radius with a representative forming trial. |
Inspection and acceptance: Match grade, heat/lot and certificate to the order. Inspect dimensions, finish, condition and markings under the agreed sampling plan. Define measurement method, tolerance and supplementary tests before order acceptance.
State S43000, ASTM editions, plate dimensions, condition, finish, tolerances, inspection and heat/lot certificate.
| Standard / designation | Grade designation | Product scope | Procurement caveat |
|---|---|---|---|
| ASTM A240/A240M | 430 / UNS S43000 | Plate thickness, cut size and supply condition. | Ferritic S43000 properties must match the delivered form and condition. |
| ASTM A480/A480M | 430 plate general requirements | Flat-product dimensions, workmanship, finish and inspection where invoked. | Define flatness, machining stock and any through-thickness examination. |
Yes. 430 is ferritic and normally magnetic; forming and product condition may influence response.
Not automatically. Compare chloride, moisture, pollutants, cleaning and finish; 430 has lower corrosion margin in many environments.
The ordered grade, ASTM A240 edition, thickness, condition and heat-specific certificate govern acceptance.
The cited ATI plate page publishes a maximum hardness; the purchase specification and ordered product condition control.
Thickness, size, finish, condition, tolerances, quantity, certificate and delivery destination.
Include the ordered grade, product form, governing specification and required inspection evidence.
Illustrative RFQ checklist, not a customer case: 430 plate grade; ASTM A240 edition; thickness and cut size; finish/temper; tolerances; application exposure; certificate and packaging.
State moisture, chloride, cleaning and temperature exposure.
Define finish, temper, thickness and forming route.
Agree dimensional, visual and certificate checks.
ATI publishes the displayed composition and mechanical limits for 430 sheet/strip. Its technical literature describes the broader grade and notes plate availability, but the numeric table shown here remains a screening reference rather than plate-specific acceptance data.
ATI page publishes sheet/strip values; use them only for grade screening and confirm plate-specific requirements and MTR.
Confirm the current edition, plate dimensions, condition and supplementary requirements.
State the active order edition, units and applicable supplements.
State thickness, width × length, finish, temper, edge, flatness and tolerances. Verify 430 plate sizes against the order basis and the chosen finish. When comparing a 430 plate supplier, require a 430 plate specification to ASTM A240, finish callout, certificate and dimensional tolerances.
Product-specific review: Attach the drawing and state specification, dimensions, condition, finish, quantity, inspection requirements and certificate.