ATI 409 HP ferritic stainless sheet data below are for UNS S40930, not every 409-family variant. Confirm the exact UNS grade, Ti/Cb balance, sheet tolerances, finish and ordered specification.

Review technical resources
Grade: 409 / UNS S40930
Product form: Sheet
Order-specific data and limits stated
Replace with an approved product-form photo

Is 409 Sheet right for the order?

Stabilized ferritic grade; exact UNS variant and forming/welding procedure govern applicability.

Stabilized ferritic grade; exact UNS variant and forming/welding procedure govern applicability.
Best for

Sheet applications

Sheet enquiries that identify the 409 HP UNS variant and define forming, weld, temperature and corrosion requirements.

Not recommended without review

Conditions that can exceed the grade margin

Do not treat 409 as chloride-pitting resistant or transfer S40930 data to another 409 variant without checking chemistry and specification.

Material identification

Grade 409

UNS S40930; EN . Verify the ordered product standard and certificate.

409 Sheet chemistry and property reference

ATI's 409 HP sheet table is explicitly for UNS S40930. It is not a blanket specification for S40900/S40910/S40920; verify the exact grade and heat certificate.

Composition limits transcribed from ATI 409 HP product data (sheet; UNS S40930). Confirm exact UNS variant and heat analysis on the material test report. Mechanical basis: ATI 409 HP product data (sheet; UNS S40930). The table states product form, condition and published limits; confirm the ordered specification and certificate.

Chemical composition by mass

ElementMinimumMaximumUnit
Cr10.5011.70wt %
Si—1.00wt %
Mn—1.00wt %
Ti0.050.75wt %
Ni—0.50wt %
P—0.040wt %
N—0.030wt %
C—0.030wt %
S—0.020wt %
Ti+Cb[0.08+8×(C+N)]0.75wt %
FeBalance—wt %

Mechanical properties

PropertyMinimumMaximum / rangeUnitCondition / reference
Tensile strength380—MPaATI 409 HP sheet; UNS S40930; minimum
0.2% yield strength170—MPaATI 409 HP sheet; UNS S40930; minimum
Elongation20—%ATI 409 HP sheet; UNS S40930; minimum
Hardness—88HRBATI 409 HP sheet; UNS S40930; maximum

Typical physical properties

PropertyPublished valueBasis / note
Density7.75 g/cm3ATI current ATI 409 HP sheet product table; UNS S40930 reference.
Mean thermal expansion, 20-100 C10.52 x 10^-6 /CATI 409 HP technical data; typical reference over stated interval, not a design value.
Specific heat at 20 C477 J/(kg K)ATI 409 HP technical data; typical reference.
Thermal conductivity, 20-100 C25.0 W/(m K)ATI 409 HP technical data; typical reference over stated interval.
Elastic modulus at 20 C200 GPaATI 409 HP technical data; typical reference, not a design allowable.
Electrical resistivity60 microohm cmATI 409 HP technical data; typical reference.

Data note: These values are material-screening references. The governing product specification, ordered condition, dimensions and heat-specific certificate determine acceptance. Review the technical resources for the applicable purchasing basis.

Replace with an approved material inspection photo

How to specify 409 Sheet

Request exact thickness, width, length, flatness, edge, finish, tolerance and coil/flat delivery form.

Duty / itemStarting optionAdvantageLimitationAlternative / action
Exhaust sheet screening409 HP sheet with exact UNS variant statedATI documents sheet forming and automotive exhaust use.Hot-end temperature and localized corrosion may exceed the grade's suitability.Evaluate a higher-alloy grade against the service conditions.
Variant selectionState UNS S40930 or another required variantPrevents chemistry/stabilization ambiguity.Type 409 naming alone may not identify Ti/Cb limits.Reconcile purchase order, product specification and heat certificate.
Formed part acceptanceDefine thickness, radii, edges and weld criteriaMakes fabrication and inspection basis reviewable.ATI product reference is not a part-specific forming approval.Qualify the process on the actual drawing and service.

Product standard: ATI lists ASTM A240 and ASME SA-240 for ATI 409 HP. The chemistry and properties displayed here are its UNS S40930 sheet data; confirm edition, grade and ordered requirements.
Finish and condition: Specify the required finish and acceptance criteria; appearance alone does not establish grade or dimensions.

Order checks: confirm exact dimensional basis, tolerance, finish, edge/end preparation, quantity and delivery requirements before quotation.

Where 409 Sheet may fit

Ferritic sheet for applications where the specified 409 variant, forming route and service environment are suitable.

ATI documents ATI 409 HP for formed sheet uses including automotive exhaust components. Suitability depends on exact UNS variant, thickness, temperature, weld route and corrosion exposure.

Automotive exhaust sheet components

ServiceConsider a specified 409 HP sheet variant for exhaust parts where environment and temperature are within the selected design basis.
Starting gradeATI 409 HP sheet; identify UNS S40930 or other required variant
Why it worksATI documents extensive 409 HP exhaust-system use and sheet forming.
LimitsATI warns chloride pitting/crevice resistance is low; hot-end service may need a higher-alloy alternative.
MaintenanceInspect formed/welded zones and verify heat/lot chemistry and corrosion exposure.

Formed sheet enclosures or components

ServiceDefine thickness, blank geometry, bend radii, edge condition and weld route before forming.
Starting grade409 HP sheet to its ordered ASTM A240 grade/variant
Why it worksATI describes 409 HP sheet as routinely bent, sheared, blanked, punched and stretch-formed.
LimitsForming depends on thickness and variant; plate guidance must not be transferred to thin sheet.
MaintenanceInspect cut edges, formed radii, weld heat-affected zones and finish.

Heat-exchanger or equipment sheet

ServiceScreen after checking process medium, temperature, fabrication and inspection needs.
Starting gradeSpecify exact 409 HP UNS variant and product form
Why it worksATI lists applications including heat-exchanger tubing and other equipment components.
LimitsThe cited product page does not qualify the grade for a specific process-fluid environment.
MaintenanceReview service corrosion and weld requirements; verify certificate and dimensions.

Risks to control for 409 Sheet

Failure modeTypical triggerControl / verification
409 UNS variant is unspecifiedA240 Type 409 is ordered without stating required variant or supplementary chemistry.Name the UNS designation and confirm carbon/Ti/Cb stabilization against the heat certificate.
Sheet and plate guidance are mixedThin-sheet data are applied to thick-gauge plate or vice versa.Match thickness and product form to the specific source table and purchase specification.
Chloride or hot-end service is underestimatedNominal 11% chromium is treated as immunity to localized corrosion or high-temperature oxidation.Assess actual medium and temperature; ATI notes limited chloride pitting/crevice resistance and higher-alloy grades may be needed for hot zones.

Inspection and acceptance: Check UNS S40930 designation, heat certificate, Ti/Cb analysis, thickness/width, surface and required tests against the purchase order.

409 Sheet standards and designation

ATI lists ASTM A240 and ASME SA-240 for ATI 409 HP. The chemistry and properties displayed here are its UNS S40930 sheet data; confirm edition, grade and ordered requirements.

Standard / designationGrade designationProduct scopeProcurement caveat
ASTM A240/A240MType 409; confirm exact UNS and editionSheetATI lists for 409 HP sheet; values shown are UNS S40930.
ASME SA-240Only if specified and applicableSheetATI lists for 409 HP; confirm code and ordered grade.

Questions about 409 stainless steel Sheet

Which 409 grade do these numbers describe?

ATI states the displayed sheet chemistry and properties are for UNS S40930; Ti/Cb ranges vary for S40910 and S40920.

What mechanical limits are published for S40930 sheet?

ATI lists tensile strength at least 380 MPa, yield strength at least 170 MPa, elongation at least 20%, and hardness no more than 88 HRB.

Can 409 sheet be substituted for 304?

Not without reviewing corrosion, forming, weld, temperature and service requirements; ferritic 409 and austenitic 304 are different alloy families.

Does this page specify sheet thickness or finish?

No stock dimensions are asserted here. Put thickness, width, length, finish, tolerances, quantity and certificate requirements in the enquiry.

What should be checked on receipt?

Match UNS grade, heat/lot certificate and ordered specification; inspect dimensions, finish, condition, markings and agreed tests.

Example: prepare a 409 Sheet enquiry

Illustrative buying case: a fabricator requests S40930 sheet with drawing dimensions, finish, tolerances and certificate requirements.

Illustrative buying case: a fabricator requests S40930 sheet with drawing dimensions, finish, tolerances and certificate requirements.

Identify variant

UNS grade and stabilization

State Type 409/UNS variant, ASTM A240 edition, and any Ti/Cb or carbon requirements.

Define sheet supply

Gauge, finish and forming basis

Specify thickness, width, flatness, edge, finish, tolerances, delivery form, quantity and certificate.

Confirm service fit

Weld, temperature and corrosion review

Provide service environment and fabrication route; agree inspection criteria for formed and welded areas.

Acceptance: Check UNS S40930 designation, heat certificate, Ti/Cb analysis, thickness/width, surface and required tests against the purchase order.

Official 409 Sheet data source

The chemistry and property tables are tied to the cited producer data and stated product form. Verify the ordered edition and heat-specific MTR.

01

ATI 409 HP product data (sheet; UNS S40930)

Verify ordered edition and heat-specific certificate.

02

ATI 409 HP product data (sheet; UNS S40930)

Reference values are not design allowables.

Request a 409 Sheet quote

Send the grade, standard edition, dimensions, finish, condition, quantity, destination and certificate requirements for a traceable quotation.

  • MaterialGrade 409; UNS S40930; EN
  • Product formSheet
  • DimensionsRequest exact thickness, width, length, flatness, edge, finish, tolerance and coil/flat delivery form.
  • Standard and conditionATI lists ASTM A240 and ASME SA-240 for ATI 409 HP. The chemistry and properties displayed here are its UNS S40930 sheet data; confirm edition, grade and ordered requirements.
  • Service / fabricationATI documents ATI 409 HP for formed sheet uses including automotive exhaust components. Suitability depends on exact UNS variant, thickness, temperature, weld route and corrosion exposure.
  • Inspection requirementsCheck UNS S40930 designation, heat certificate, Ti/Cb analysis, thickness/width, surface and required tests against the purchase order.

Product-specific review: Check UNS S40930 designation, heat certificate, Ti/Cb analysis, thickness/width, surface and required tests against the purchase order.