Plate applications
Plate enquiries that identify the 409 HP UNS variant and define forming, weld, temperature and corrosion requirements.
REQUEST A QUOTE
Send the details you already know. Our team can review the remaining technical points with you.
Plate · Grade 409 / S40930
409 stainless steel plate is a stabilized ferritic grade considered for automotive exhaust, heat-resistant and fabrication applications. This page uses ATI S40930 sheet/strip data for grade screening; EN 1.4512 is shown only as a 409-family reference, not as an asserted exact cross-equivalence. Confirm the plate UNS, product standard, thickness, condition and certificate.

Stabilized ferritic grade; exact UNS variant and forming/welding procedure govern applicability.
Plate enquiries that identify the 409 HP UNS variant and define forming, weld, temperature and corrosion requirements.
Do not treat 409 as chloride-pitting resistant or transfer S40930 data to another 409 variant without checking chemistry and specification.
UNS S40930; EN 1.4512 family reference. Verify the ordered product standard and certificate.
Chemistry and physical values are S40930 grade references; the mechanical table is explicitly sourced to ATI sheet/strip data. Plate acceptance requires the ordered product specification and MTR.
ATI 409 HP S40930 composition limits are shown as a grade reference. Confirm the ordered plate UNS variant and heat analysis. ATI publishes 380 MPa tensile, 170 MPa yield, 20% elongation and 88 HRB maximum for UNS S40930 sheet/strip. These values are screening references only and are not plate-specific acceptance limits.
| Element | Minimum | Maximum | Unit |
|---|---|---|---|
| Cr | 10.50 | 11.70 | wt % |
| Si | — | 1.00 | wt % |
| Mn | — | 1.00 | wt % |
| Ti | 0.05 | 0.75 | wt % |
| Ni | — | 0.50 | wt % |
| P | — | 0.040 | wt % |
| N | — | 0.030 | wt % |
| C | — | 0.030 | wt % |
| S | — | 0.020 | wt % |
| Ti+Cb | [0.08+8×(C+N)] | 0.75 | wt % |
| Fe | Balance | — | wt % |
| Property | Minimum | Maximum / range | Unit | Condition / reference |
|---|---|---|---|---|
| Tensile strength | 380 | — | MPa | ATI 409 HP sheet/strip, UNS S40930; published minimum. Screening reference for a plate enquiry only. |
| 0.2% yield strength | 170 | — | MPa | ATI 409 HP sheet/strip, UNS S40930; published minimum. Screening reference for a plate enquiry only. |
| Elongation | 20 | — | % | ATI 409 HP sheet/strip, UNS S40930; published minimum. Screening reference for a plate enquiry only. |
| Hardness | — | 88 | HRB | ATI 409 HP sheet/strip, UNS S40930; published maximum. Screening reference for a plate enquiry only. |
| Property | Published value | Basis / note |
|---|---|---|
| Density | 7.75 g/cm3 | ATI current ATI 409 HP sheet product table; UNS S40930 reference. |
| Mean thermal expansion, 20-100 C | 10.52 x 10^-6 /C | ATI 409 HP technical data; typical reference over stated interval, not a design value. |
| Specific heat at 20 C | 477 J/(kg K) | ATI 409 HP technical data; typical reference. |
| Thermal conductivity, 20-100 C | 25.0 W/(m K) | ATI 409 HP technical data; typical reference over stated interval. |
| Elastic modulus at 20 C | 200 GPa | ATI 409 HP technical data; typical reference, not a design allowable. |
| Electrical resistivity | 60 microohm cm | ATI 409 HP technical data; typical reference. |
Data note: These values are material-screening references. The governing product specification, ordered condition, dimensions and heat-specific certificate determine acceptance. Review the technical resources for the applicable purchasing basis.

Request exact thickness, width, length, flatness, edge, finish, tolerance and coil/flat delivery form.
| Duty / item | Starting option | Advantage | Limitation | Alternative / action |
|---|---|---|---|---|
| Exhaust plate screening | 409 HP plate with exact UNS variant stated | ATI documents plate forming and automotive exhaust use. | Hot-end temperature and localized corrosion may exceed the grade's suitability. | Evaluate a higher-alloy grade against the service conditions. |
| Variant selection | State UNS S40930 or another required variant | Prevents chemistry/stabilization ambiguity. | Type 409 naming alone may not identify Ti/Cb limits. | Reconcile purchase order, product specification and heat certificate. |
| Formed part acceptance | Define thickness, radii, edges and weld criteria | Makes fabrication and inspection basis reviewable. | ATI product reference is not a part-specific forming approval. | Qualify the process on the actual drawing and service. |
Product standard: ATI lists ASTM A240/ASME SA-240 for ATI 409 HP flat product. State the exact UNS variant, edition, plate dimensions, condition, surface, tests and certification.
Finish and condition: Specify the required finish and acceptance criteria; appearance alone does not establish grade or dimensions.
Order checks: confirm exact dimensional basis, tolerance, finish, edge/end preparation, quantity and delivery requirements before quotation.
Ferritic plate for applications where the specified 409 variant, forming route and service environment are suitable.
ATI documents ATI 409 HP for formed plate uses including automotive exhaust components. Suitability depends on exact UNS variant, thickness, temperature, weld route and corrosion exposure.
| Failure mode | Typical trigger | Control / verification |
|---|---|---|
| 409 UNS variant is unspecified | A240 Type 409 is ordered without stating required variant or supplementary chemistry. | Name the UNS designation and confirm carbon/Ti/Cb stabilization against the heat certificate. |
| Plate and plate guidance are mixed | Thin-plate data are applied to thick-gauge plate or vice versa. | Match thickness and product form to the specific source table and purchase specification. |
| Chloride or hot-end service is underestimated | Nominal 11% chromium is treated as immunity to localized corrosion or high-temperature oxidation. | Assess actual medium and temperature; ATI notes limited chloride pitting/crevice resistance and higher-alloy grades may be needed for hot zones. |
Inspection and acceptance: Check UNS S40930 designation, heat certificate, Ti/Cb analysis, thickness/width, surface and required tests against the purchase order.
State the exact UNS variant, plate product specification, edition, dimensions, condition, tests and certification. EN 1.4512 is a 409-family reference and must not be treated as an automatic exact equivalent to UNS S40930.
| Standard / designation | Grade designation | Product scope | Procurement caveat |
|---|---|---|---|
| ASTM A240/A240M | 409 / UNS S40930 | Plate thickness, cut size and supply condition. | Order the exact S40930 variant and stabilization limits rather than generic 409 chemistry. |
| ASTM A480/A480M | 409 plate general requirements | Flat-product dimensions, workmanship, finish and inspection where invoked. | Define flatness, machining stock and any through-thickness examination. |
ATI states the displayed plate chemistry and properties are for UNS S40930; Ti/Cb ranges vary for S40910 and S40920.
ATI lists tensile strength at least 380 MPa, yield strength at least 170 MPa, elongation at least 20%, and hardness no more than 88 HRB.
Not without reviewing corrosion, forming, weld, temperature and service requirements; ferritic 409 and austenitic 304 are different alloy families.
No stock dimensions are asserted here. Put thickness, width, length, finish, tolerances, quantity and certificate requirements in the enquiry.
Match UNS grade, heat/lot certificate and ordered specification; inspect dimensions, finish, condition, markings and agreed tests.
Illustrative buying case: a fabricator requests S40930 plate with drawing dimensions, finish, tolerances and certificate requirements.
Illustrative buying case: a fabricator requests S40930 plate with drawing dimensions, finish, tolerances and certificate requirements.
State Type 409/UNS variant, ASTM A240 edition, and any Ti/Cb or carbon requirements.
Specify thickness, width, flatness, edge, finish, tolerances, delivery form, quantity and certificate.
Provide service environment and fabrication route; agree inspection criteria for formed and welded areas.
ATI S40930 sheet/strip data support grade screening. ASTM A240 supplies the flat-product route, but the producing mill must confirm plate availability, thickness-specific requirements and certification.
Sheet values support screening only; verify plate form, thickness and heat certificate.
Confirm exact UNS variant, ordered edition, plate condition and supplements.
Use when invoked by the accepted product specification or purchase order.
Send the grade, standard edition, dimensions, finish, condition, quantity, destination and certificate requirements for a traceable quotation.
Product-specific review: Check UNS S40930 designation, heat certificate, Ti/Cb analysis, thickness/width, surface and required tests against the purchase order.