Sheet applications
Sheet components requiring a defined age-hardening condition and a qualified balance of strength, toughness and corrosion resistance.
REQUEST A QUOTE
Send the details you already know. Our team can review the remaining technical points with you.
Sheet · Grade 17-4 PH / S17400
17-4 PH stainless steel sheet (UNS S17400 / Type 630) is a precipitation-hardening alloy supplied solution-annealed and aged to selected strength/toughness conditions. State the exact condition; the H900 figures below are not solution-annealed delivery values.

Share the service environment and design basis for review.
Sheet components requiring a defined age-hardening condition and a qualified balance of strength, toughness and corrosion resistance.
Do not specify only “17-4 PH.” H900, H1025 and H1150 conditions yield different properties; do not substitute ASTM A564 bar values for A693 sheet.
UNS S17400; EN 1.4542. Verify the ordered product standard and certificate.
The H900 condition data are not the solution-annealed supply condition. Age treatment changes strength and toughness; specify the required condition and verify the corresponding A693/AMS certificate.
ATI producer chemistry for sheet/strip/plate UNS S17400. Cb is niobium (Nb); confirm the ordered standard and heat analysis. Mechanical values below are ATI sheet H900 heat-treated values: tensile ≥1310 MPa, yield ≥1172 MPa, elongation ≥5%, hardness 40–47 HRC. ATI typically supplies solution-annealed sheet with max 38 HRC; do not confuse these conditions.
| Element | Minimum | Maximum | Unit |
|---|---|---|---|
| C | — | 0.07 | wt % |
| Mn | — | 1.00 | wt % |
| Si | — | 1.00 | wt % |
| P | — | 0.040 | wt % |
| S | — | 0.030 | wt % |
| Cr | 15.00 | 17.50 | wt % |
| Ni | 3.00 | 5.00 | wt % |
| Cu | 3.00 | 5.00 | wt % |
| Cb/Nb | 0.15 | 0.45 | wt % |
| Fe | Balance | — | wt % |
| Property | Minimum | Maximum / range | Unit | Condition / reference |
|---|---|---|---|---|
| Tensile strength — H900 | 1310 | — | MPa | ATI sheet H900 minimum; aged condition only. |
| 0.2% yield strength — H900 | 1172 | — | MPa | ATI sheet H900 minimum; aged condition only. |
| Elongation — H900 | 5 | — | % | ATI sheet H900 minimum. |
| Hardness — H900 | 40 | 47 | HRC | ATI sheet H900 range. |
| Hardness — solution annealed supply condition | — | 38 | HRC | ATI typical supply maximum; not the H900 value. |
| Property | Published value | Basis / note |
|---|---|---|
| Density — Condition A | 7.75 g/cm³ | ATI typical Condition A physical property. |
| Thermal expansion, −73 to +21°C — Condition A | 11.3 × 10⁻⁶ /°C | ATI typical value over the stated temperature interval. |
| Thermal conductivity, 21–100°C — Condition A | 18.3 W/(m·K) | ATI typical Condition A value over the stated interval. |
| Elastic modulus — Condition A | 196 GPa | ATI typical mechanical reference. |
| Electrical resistivity — Condition A | 98 μΩ·cm | ATI typical Condition A physical property. |
Data note: These values are material-screening references. The governing product specification, ordered condition, dimensions and heat-specific certificate determine acceptance. Review the technical resources for the applicable purchasing basis.

Specify sheet thickness, width/length, finish, edge, solution-annealed delivery condition, age condition, flatness, tolerances, test coupons and certification.
| Duty / item | Starting option | Advantage | Limitation | Alternative / action |
|---|---|---|---|---|
| High-strength sheet component | 17-4 PH solution-annealed sheet, age after forming | Aging can produce high strength in a defined condition. | Post-age distortion and reduced ductility require validation. | Set H900/H1025/H1150 condition, shape and test basis. |
| Form-before-age fabrication | Solution-annealed sheet with qualified forming route | ATI identifies solution-annealed supply condition. | Springback and age-treatment distortion affect tolerances. | Provide formed geometry, allowance and furnace route. |
| Corrosion plus stress | Select age condition based on environment and stress | Precipitation hardening provides strength with moderate corrosion resistance. | Not equivalent to 316L; stress-corrosion response varies with condition. | Provide chloride, temperature, stress and inspection plan. |
Product standard: ATI lists ASTM A693/ASME SA-693 and AMS 5604 for 17-4 PH sheet/strip/plate. ASTM A480/A480M general flat-product requirements may apply when invoked.
Finish and condition: Specify finish, roughness, edge preparation and cleaning route; appearance alone does not establish grade or acceptance.
Order checks: confirm exact dimensional basis, tolerance, finish, edge/end preparation, quantity and delivery requirements before quotation.
Share dimensions and service conditions for product-form review.
Define as-supplied solution-annealed or final aged condition, forming before aging, age temperature/time, final hardness, section and service temperature.
| Failure mode | Typical trigger | Control / verification |
|---|---|---|
| Condition confusion | H900 minima represented as solution-annealed values. | Label every value with condition and age cycle. |
| Wrong standard/form | A564 bar property data substituted for A693 sheet. | Use flat-product requirements for sheet. |
| Age-induced distortion | No dimensional allowance for precipitation hardening. | Plan machining sequence and post-age inspection. |
| Corrosion overclaim | Strength grade assumed equivalent to 316L. | Evaluate chemistry, surface, medium and stress. |
Inspection and acceptance: Match ordered grade, product form, condition, heat/lot and certificate; inspect dimensions, surface and markings under the agreed inspection plan.
ATI lists ASTM A693/ASME SA-693 and AMS 5604 for 17-4 PH sheet/strip/plate. ASTM A480/A480M general flat-product requirements may apply when invoked.
| Standard / designation | Grade designation | Product scope | Procurement caveat |
|---|---|---|---|
| ASTM A693/A693M | 17-4 PH / UNS S17400 | 17-4 PH / UNS S17400 — Precipitation-hardening stainless plate, sheet and strip. | State solution/aged condition and current edition. |
| AMS 5604 | 17-4 PH / UNS S17400 | 17-4 PH sheet/strip/plate — Aerospace product specification listed by ATI. | Verify AMS edition and supplemental requirements. |
| ASTM A480/A480M | 17-4 PH / UNS S17400 | General flat-product requirements — Dimensional/general requirements where invoked. | Does not replace the A693 grade/condition requirements. |
ATI says 17-4 sheet is typically supplied solution annealed, with hardness maximum 38 HRC.
The 1310 MPa tensile and 1172 MPa yield minima shown here are for ATI H900 heat-treated sheet, not solution-annealed stock.
ATI lists ASTM A693/ASME SA-693 and AMS 5604; use the standard and edition written on the order.
Forming route depends on condition and geometry; ATI describes solution-annealed delivery followed by age hardening. Qualify forming before aging and final distortion.
No. Lower aging temperatures raise strength but may reduce toughness; select condition against stress, impact, corrosion and temperature.
Provide dimensions, condition, quantity and destination for quotation.
Illustrative enquiry: 17-4 PH Sheet; state standard and edition, dimensions, condition, quantity, destination and certificate.
State UNS S17400, ASTM A693 or AMS 5604 edition, thickness, finish and condition.
Choose H900 or alternate aging condition from qualified design data.
Check heat chemistry, condition, tensile/hardness tests, furnace record and post-age dimensions.
Producer and standards references are listed below. Confirm current edition, scope and heat/lot certificate before acceptance.
Official sheet/strip/plate form, chemistry, H900 properties and solution-annealed supply note. Source URL: https://www.atimaterials.com/Products/Pages/ati-17-4.aspx
Official precipitation-hardening stainless plate, sheet and strip specification scope. Source URL: https://store.astm.org/a0693-22.html
General flat-product dimensional/quality requirements where invoked. Source URL: https://www.astm.org/a0480_a0480m.html
Producer technical data and heat-treatment guidance. Official ATI technical datasheet v2. Source URL: https://www.atimaterials.com/Products/Documents/datasheets/stainless-specialty-steel/precipitationhardening/ati_17-4_tds_en_v2.pdf